Long-term development of mechanical properties of concrete with different water to cement ratio and internal curing ability
Concretes with water to cement (or binder) ratios of Jewelry Dish 0.50.0.40, 0.30 and 0.20 were prepared and long-term mechanical properties were measured.Porous light-weight aggregates (LWA) in dosages of 10 % and 20 % were used for self-curing (internal curing) as a partial replacement of fine aggregates for some concrete types.Two environmental